When the forging burr scale exceeds the forging skill condition; it is ground on the grinding wheel; and usually before the forging is annealed.
Forgings yttrium oxide is usually carried out after annealing; there are two types of horizontal drum finishing and shot blasting finishing:
1. Horizontal drum finishing: Many bearing rings with different scales are loaded together into a horizontal drum that reverses at a speed of 20-60r/min and smashed and hit each other; the cerium oxide is dropped from the surface of the forging; together It can polish the burrs and edges of the forgings; in order to speed up the finishing; sometimes put some scrap balls in the drum. The finishing time is usually 10~20min. This method is simple and easy; but the finishing quality is poor.
2. Shot blasting finishing: loading the forging into a horizontal sealing drum that is converted at a low speed (2.5 to 3r/min); iron or steel pellets with a particle size of 0.8 to 1.2 mm; The blade is thrown and rushed onto the forging; the cerium oxide is dropped by the impact. The steel pellet can be actively circulated; the cerium oxide is sucked out by the vacuum cleaner; the forging impact noise is small.
Recommend to friends comments close window
Bearing related knowledge |
Common terms and definitions of bearings (3) Ways to determine whether NTN bearings are available Causes of noise in NSK bearings and treatment methods Excavator bearing device and disassembly method Combined rolling bearing improves spindle speed (2) |
This article links to http://
Please indicate China Bearing Network http://
Previous:How to eradicate the oil stain on the INA bearing Next:The correct use of the rolling bearing and the cause of the problem
Bulkhead Light,Flood Led Light,Flood Lights,Led Flood Light
JIANGMEN MOSCOT OPTOELECTRONIC TECHNOLOGY CO.,LTD. , https://www.jmsensorsled.com